Induction Brass Melting Furnace
Induction Brass Melting Furnace | SMJD Series, 500-3,000 kg Copper & Brass per Heat
The induction brass melting furnace on this page is HLQ’s SMJD series medium frequency induction melting furnace, supplied in thirteen sizes from SMJD-463 to SMJD-3100. It melts 500 kg to 3,000 kg of copper, gold and silver scrap and slag per heat from 60 kW to 200 kW input on a 3-phase 380 V, 50-60 Hz supply, with oscillation frequency published from 1 kHz to 100 kHz and a custom frequency available on request, and a maximum furnace temperature of 1800 °C. It is an electric furnace with IGBT power devices: no burner, no fuel, no combustion exhaust. Every figure on this page is published by HLQ in the SMJD parameter sheet, the manufacturer’s manual or HLQ’s own brass and copper references, and is reproduced here with its source.
The three official documents behind this page are the SMJD induction melting furnace parameter sheet, the Aluminum, Copper, Iron induction melting furnace manual, and the aluminum scraps recycling melting process note.
Quick Answer
An induction brass melting furnace is an electric furnace that melts brass, bronze and copper alloys by generating the heat inside the metal itself, with no flame anywhere near the melt. The SMJD series covers thirteen sizes with a published brass, copper, gold and silver capacity of 500 kg per heat at SMJD-463 rising to 3,000 kg at SMJD-3100, from 60 kW to 200 kW input with published input current of 90 A to 300 A, a 3-phase 380 V 50-60 Hz supply, and a maximum furnace temperature of 1800 °C. The power devices are IGBT, with digital phase locked loop frequency tracking, automatic load impedance matching, closed-loop power control, PID heating control and an LED digital controller accurate to 3 °C, and the load duration is 100 % for 24 hours.
Brass is not copper with a different label, and the process control is the reason. HLQ publishes the brass melting range at about 885-955 °C depending on grade, and zinc boils at 907 °C, so zinc loss is the main process risk rather than a secondary one. The published controls are a melt held at 950-1,020 °C and never above 1,050 °C, short holding time, zinc added as the last element, a flux cover kept on the melt, and fume extraction running throughout the heat. The vessel follows the metal: brass is published with a silica lining, SiO₂ ≥ 97 %, sintered at 1,050-1,100 °C, with an expected life of 200-400 heats.
There is one scope point worth stating plainly. The published SMJD capacity table this page links to has three columns — steel and stainless steel, then copper, gold and silver (scrap, slag), then aluminum, aluminum alloy, aluminum scrap, aluminum slag and pop can. Neither brass nor bronze is named in that table, and the brass figure for a buyer comes from the second column, the copper and precious-metals one. The small-batch brass system with its own silica-lining protocol is published separately on HLQ’s induction melting brass page, and the larger induction copper melter range covers the 100 kg to 1,000 kg class.
Table of Contents
- Quick Answer
- Table of Contents
- What is the Brass Melting Furnace?
- Key Applications
- Suitable Materials
- Working Principle
- Technical Specifications
- Recommended Model Selection
- Process Workflow
- Common Problems and Solutions
- Engineering Selection Guide
- Advantages and Limitations
- Why Choose HLQ?
- 6 Core FAQs
What is the Brass Melting Furnace?
A brass melting furnace is a batch melting furnace that brings copper-zinc and copper-tin alloys to a liquid state and pours them into a ladle or a mould. In the trade the same machine is called an induction brass furnace, a copper smelter, a bronze melting furnace or a copper melting induction furnace, because a single furnace body with a single crucible can carry any of the copper-alloy family once the lining and the process recipe are right.
What separates a brass furnace from a general-purpose induction furnace is that the alloy decides the process, and the alloy is unforgiving in a way that aluminium is not. Brass melts about 885-955 °C depending on grade, and zinc boils at 907 °C. A melt held too hot, or held too long, loses zinc, and the casting then misses its specification. A melt held correctly still needs a flux cover and a fume hood. Those three facts — the temperature window, the flux cover and the extraction — are what this page is organised around.
Physically the machine is a steel-shell furnace with an integral refractory lining, a water-cooled copper induction coil, a crucible sized for the alloy, a tilting mechanism for the pour, and a separate medium frequency power supply with its capacitor cabinet. The crucible is the susceptor, the container and a consumable, and its chemistry has to match the alloy family, because the published rule is that a lining used for brass must not be used for pure copper: zinc absorbed in the lining can contaminate the copper.
The small-batch brass system with its own silica-lining protocol and its own twelve-step sequence is published on HLQ’s induction melting brass page, and the larger industrial reference is the 5000 kg copper melting induction furnace range. This page is the scope and selection reference: which alloy, which lining, and what the published capacity table actually covers.
Key Applications
HLQ publishes the brass and copper applications with the alloy grades, the capacity and the single requirement that decides the specification for each one. That last column is the useful one, because it tells a buyer what has to be true before the application is viable.
| Application | Alloys | Capacity | Key requirement |
|---|---|---|---|
| Brass valve and fitting production | C36000, C28000, C37700 | 200-1,000 kg | Zinc-loss control, fast cycle, consistent chemistry |
| Small brass foundry | C26000, C36000 | 100-300 kg | Zinc-loss control; fume extraction |
| Medium brass / bronze foundry | C28000, C90500 | 300-1,000 kg | Hydraulic tilt; PLC control; batch production |
| Laboratory and small casting | All copper alloys | 5-100 kg | Flexible alloy switching |
| Brass scrap recycling | Sorted brass scrap | By project | Sorting and drying; zinc recovery by vacuum distillation |
Four things follow from that table, and they are the practical shape of a brass plant.
Zinc-loss control is the first requirement on every brass application, not the last one. The same control applies whether the charge is a clean C36000 billet or sorted scrap, because the risk is in the melt, not in the feed. That is why the published melt window, the “add zinc last” rule and the flux cover appear in every brass process, and why fume extraction is listed as a key requirement rather than a nice-to-have.
The grade decides the venting. C36000 free-cutting brass carries lead, and the published handling note for it is ventilation required; the other brass grades carry zinc, and the note is zinc fuming with fume extraction. A shop that runs both needs the hood anyway, and needs to know that the lead-bearing grade is the one that turns it into a workplace issue rather than a process issue.
Alloy switching is a capability and a hazard at the same time. The published application for laboratory and small casting is flexible alloy switching, and the published limitation is that a brass lining should not be used for pure copper. One furnace, many alloys, works only with discipline about which lining and which crucible go in.
Brass scrap recycling is a different product. The published requirement is sorting and drying plus zinc recovery by vacuum distillation, because the zinc in mixed scrap does not simply melt into the ingot — it has to be recovered or it is lost. HLQ publishes the vacuum route separately as the separation and recovery zinc vacuum furnaces for copper-zinc alloy scraps, and the induction copper melting furnace page covers the induction half of the chain.
Suitable Materials
Which alloy a furnace can melt is decided by three numbers: the alloy’s melting range, its density, and the lining that resists it. HLQ publishes all three for the copper-alloy family, and the table below is the working reference for a brass shop.
| Material | Standard grade | Melting range | Density (kg/dm³) | Recommended lining | Special handling |
|---|---|---|---|---|---|
| Cartridge brass 70/30 | C26000 | 915-955 °C | 8.53 | Silica (SiO₂ ≥ 97 %) | Zinc fuming; fume extraction required |
| Muntz metal 60/40 brass | C28000 | 900-940 °C | 8.39 | Silica | Higher zinc loss; temperature control critical |
| Free-cutting brass | C36000 | 885-900 °C | 8.50 | Silica or alumina-silica | Lead content; ventilation required |
| Tin bronze (gunmetal) | C90300, C90500 | 850-1,000 °C | 8.80 | Silica or alumina | Phosphorus deoxidation standard |
| Bearing bronze | C93200 (SAE 660) | 854-1,000 °C | 8.93 | Silica | Lead segregation risk; stir well |
| Aluminum bronze | C95400, C95500 | 1,030-1,100 °C | 7.45 | Alumina (Al₂O₃ ≥ 90 %) | Al₂O₃ inclusion control; careful skimming |
| Silicon bronze | C65500 | 970-1,025 °C | 8.53 | Silica or alumina | Good fluidity; low gas absorption |
| Electrolytic tough pitch copper | Cu-ETP (C11000) | 1,083-1,100 °C | 8.96 | Magnesia (MgO ≥ 90 %) | Oxygen control; charcoal cover |
| Oxygen-free copper | Cu-OF (C10200) | 1,083-1,095 °C | 8.94 | Magnesia or alumina-magnesia | Inert gas blanket mandatory |
| Brass returns and scrap | Sorted by alloy | Varies | Bulk 2-5 kg/dm³ | Match to the dominant alloy | Pre-sort, pre-dry, manage dross |
Two things in that table are worth pausing on. First, the density column: brass runs 8.39-8.53 kg/dm³ and copper 8.94-8.96, so this is one of the densest common metal families and the charge has real thermal mass. Second, the scrap row: bulk density falls to 2-5 kg/dm³ for returns, which is a quarter of solid metal density, and that is the reason scrap melting is a longer, lower-density and more dross-intensive duty than ingot melting on the same furnace.
The lining is not a detail on this equipment, it is a consumable with a chemistry, a sintering schedule and a service life, and HLQ publishes the matrix by alloy family.
| Alloy family | Recommended lining | Content | Sintering temperature | Expected life (heats) | Primary failure mode |
|---|---|---|---|---|---|
| Brass (Cu-Zn) | Silica (acid) | SiO₂ ≥ 97 % | 1,050-1,100 °C | 200-400 | Thermal cycling erosion |
| Pure copper (ETP, OF, OFE) | Magnesia (basic) | MgO ≥ 90 % | 1,150-1,200 °C | 150-350 | Cu₂O chemical attack on silica |
| Tin bronze (Cu-Sn) | Silica or alumina | SiO₂ ≥ 95 % or Al₂O₃ ≥ 85 % | 1,050-1,150 °C | 180-350 | SnO₂ flux penetration |
| Aluminum bronze (Cu-Al) | Alumina (neutral) | Al₂O₃ ≥ 90 % | 1,100-1,200 °C | 120-280 | Al₂O₃ inclusion buildup |
| Cupronickel (Cu-Ni) | Chrome-magnesia or spinel | MgO ≥ 70 % + Cr₂O₃ ≥ 15 % | 1,200-1,280 °C | 100-250 | High-temperature creep and spalling |
| Beryllium copper | High-purity alumina | Al₂O₃ ≥ 95 % | 1,100-1,150 °C | 100-200 | BeO reaction with basic linings |
Read the two brass rows together and the rule is visible: brass takes an acidic silica lining and pure copper takes a basic magnesia lining, and the published failure modes are each other’s hazard — copper attacks silica chemically, and silica is what brass needs. That is why the published selection factor is a lining dedicated to brass or shared with other alloys, with a separate lining kept for pure copper, and why a dedicated lining or furnace for each alloy family appears in the troubleshooting reference.
Working Principle
HLQ describes the working principle of this machine in its own manual, and the version for a copper alloy reads the same as the version for aluminium until it reaches the temperature.
“Electromagnetic melting furnaces use electromagnetic induction heating to convert electrical energy into thermal energy through an electromagnetic induction heating controller. First of all, through the internal rectifier filter circuit to AC power into DC, and then through the control circuit to convert DC power into high-frequency magnetic energy. High-speed changing current through the coil will produce a high-speed changing magnetic field. When the magnetic field lines in the magnetic field pass through the crucible, numerous small eddy currents will be generated inside the crucible, so that the crucible itself is heated at a high speed, and the heat will be transferred to the aluminum alloy and melted into a liquid state.”
Three points in that chain decide whether a brass melt is good. The **field passes through the crucible**, so the crucible is the susceptor and it is a consumable whose chemistry has to match the alloy. The **rotating field stirs the bath**, and for brass that is what keeps the zinc evenly distributed through the melt rather than stratified through it. And the **control stage tracks the load**, which on a brass duty is the difference between holding 950 °C and drifting towards 1,050 °C, where the zinc starts leaving the melt.
The consequence is a narrow, published operating window, and HLQ states it plainly: brass melts at about 885-955 °C depending on grade, zinc boils at 907 °C, so zinc loss is the main process risk. The four published controls that follow are the whole brass process in miniature.
| Control | Published requirement | Why it matters for brass |
|---|---|---|
| Melt temperature | Hold at 950-1,020 °C, never above 1,050 °C | The window above the brass melting point and below the point where zinc loss accelerates. |
| Holding time | Keep it short | Zinc leaves the melt for as long as the melt is held hot. |
| Zinc addition | Add zinc as the last element | Published to limit zinc loss to the melt. |
| Flux cover | Charcoal or copper flux, kept on during the heat | Keeps the surface covered so oxidation products are held in the flux rather than in the metal. |
| Fume extraction | A hood above the furnace, running throughout the heat | Zinc and lead fumes; the published selection factor, not an accessory. |
The published brass melt temperature recommendation is 950-1,020 °C, never above 1,050 °C, on a lining of silica with SiO₂ ≥ 97 %, sintered at 1,050-1,100 °C, with an expected life of 200-400 heats. The published maximum furnace temperature of 1800 °C is the ceiling of the furnace, not the working point: a brass melt is deliberately held two hundred degrees below it.
Technical Specifications
The following three tables are the SMJD specification sheet reproduced in full, published by HLQ in the parameter PDF linked at the top of this page. The brass-relevant figure is the middle capacity column.
1. Melting capacity of the SMJD series
| Type | Input power | Melting capacity: steel and stainless steel | Melting capacity: copper, gold, silver (scrap, slag) | Melting capacity: aluminum, aluminum alloy, aluminum scrap, aluminum slag, pop can | Max temperature |
|---|---|---|---|---|---|
| SMJD-463 | 60 kW | 200 kg | 500 kg | 200 kg | 1800 °C |
| SMJD-480 | 60 kW | 150 kg | 500 kg | 150 kg | 1800 °C |
| SMJD-580 | 80 kW | 200 kg | 600 kg | 200 kg | 1800 °C |
| SMJD-600 | 60 kW | 230 kg | 560 kg | 230 kg | 1800 °C |
| SMJD-900 | 120 kW | 300 kg | 900 kg | 300 kg | 1800 °C |
| SMJD-905 | 80 kW | 300 kg | 900 kg | 300 kg | 1800 °C |
| SMJD-1250 | 80 kW | 400 kg | 1,200 kg | 400 kg | 1800 °C |
| SMJD-1250 | 120 kW | 450 kg | 1,350 kg | 450 kg | 1800 °C |
| SMJD-1500 | 120 kW | 500 kg | 1,500 kg | 500 kg | 1800 °C |
| SMJD-1550 | 120 kW | 520 kg | 1,560 kg | 520 kg | 1800 °C |
| SMJD-1700 | 160 kW | 600 kg | 1,700 kg | 600 kg | 1800 °C |
| SMJD-2300 | 160 kW | 800 kg | 2,000 kg | 800 kg | 1800 °C |
| SMJD-3100 | 200 kW | 1,200 kg | 3,000 kg | 1,200 kg | 1800 °C |
Two points a brass buyer should take from that table. The SMJD-1250 appears twice, at 80 kW and at 120 kW, with 1,200 kg and 1,350 kg respectively, and the crucible specification lists only one SMJD-1250 crucible for both, so the two ratings share a vessel and differ in power supply. And the brass column is the middle one, running 500 kg to 3,000 kg; the third column is aluminium at 150 kg to 1,200 kg, and the first is steel. Neither brass nor bronze is named in the table heading, which is why the brass figure for a quotation is taken from the second column and confirmed against the brass-specific data on the alloy table above.
2. Main technical parameters
| Type | Output power | Input current | Input voltage | Oscillation frequency |
|---|---|---|---|---|
| SMJD-463 | 60 kW | 90 A | 3-phase 380 V, 50-60 Hz | 1 kHz – 100 kHz, custom frequency according to customer request |
| SMJD-480 | 60 kW | 90 A | 3-phase 380 V, 50-60 Hz | 1 kHz – 100 kHz, custom frequency according to customer request |
| SMJD-580 | 80 kW | 120 A | 3-phase 380 V, 50-60 Hz | 1 kHz – 100 kHz, custom frequency according to customer request |
| SMJD-600 | 60 kW | 90 A | 3-phase 380 V, 50-60 Hz | 1 kHz – 100 kHz, custom frequency according to customer request |
| SMJD-900 | 120 kW | 180 A | 3-phase 380 V, 50-60 Hz | 1 kHz – 100 kHz, custom frequency according to customer request |
| SMJD-905 | 80 kW | 120 A | 3-phase 380 V, 50-60 Hz | 1 kHz – 100 kHz, custom frequency according to customer request |
| SMJD-1250 | 80 kW | 120 A | 3-phase 380 V, 50-60 Hz | 1 kHz – 100 kHz, custom frequency according to customer request |
| SMJD-1250 | 120 kW | 180 A | 3-phase 380 V, 50-60 Hz | 1 kHz – 100 kHz, custom frequency according to customer request |
| SMJD-1500 | 120 kW | 180 A | 3-phase 380 V, 50-60 Hz | 1 kHz – 100 kHz, custom frequency according to customer request |
| SMJD-1550 | 120 kW | 180 A | 3-phase 380 V, 50-60 Hz | 1 kHz – 100 kHz, custom frequency according to customer request |
| SMJD-1700 | 160 kW | 240 A | 3-phase 380 V, 50-60 Hz | 1 kHz – 100 kHz, custom frequency according to customer request |
| SMJD-2300 | 160 kW | 240 A | 3-phase 380 V, 50-60 Hz | 1 kHz – 100 kHz, custom frequency according to customer request |
| SMJD-3100 | 200 kW | 300 A | 3-phase 380 V, 50-60 Hz | 1 kHz – 100 kHz, custom frequency according to customer request |
3. Crucible specification
| Type | Specification | Upper mouth outer diameter (A), ±10 mm | Upper mouth inner diameter (B), ±5 mm | Bottom outer diameter (C), ±10 mm | Total height (H), ±10 mm |
|---|---|---|---|---|---|
| SMJD-463 | 463# | 565 mm | 500 mm | 310 mm | 617 mm |
| SMJD-480 | 480# | 510 mm | 420 mm | 400 mm | 710 mm |
| SMJD-580 | 580# | 420 mm | 360 mm | 300 mm | 840 mm |
| SMJD-600 | 600# | 620 mm | 525 mm | 620 mm | 470 mm |
| SMJD-900 | 900# | 520 mm | 425 mm | 510 mm | 960 mm |
| SMJD-905 | 905# | 620 mm | 530 mm | 620 mm | 650 mm |
| SMJD-1250 | 1250# | 620 mm | 535 mm | 620 mm | 850 mm |
| SMJD-1500 | 1500# | 735 mm | 640 mm | 460 mm | 900 mm |
| SMJD-1550 | 1550# | 775 mm | 682 mm | 400 mm | 750 mm |
| SMJD-1700 | 1700# | 610 mm | 500 mm | 610 mm | 1200 mm |
| SMJD-2300 | 2300# | 880 mm | 775 mm | 355 mm | 1000 mm |
| SMJD-3100 | 3100# | 780 mm | 645 mm | 780 mm | 1400 mm |
4. Published features and protection
| Feature | Published specification |
|---|---|
| Power devices | IGBT power devices, high reliability, stable operation and low maintenance costs. |
| Frequency control | Digital phase locked loop tracking frequency, automatic load impedance matching. |
| Power control | Power closed-loop control, to avoid the temperature change caused by the power down. |
| Protection | Over-voltage, under-voltage, phase loss, over-current and over-heat protection; real-time display of the parameters; fault diagnosis and alarm; leakage automatic alarm, cut off the power supply and real-time display of the working state. |
| Heating control | PID heating control system, uniform heating temperature, prevents melt temperature drift, less burning and more homogeneous metal composition, improving the product qualification rate. |
| Temperature controller | LED digital temperature controller, measuring and controlling accuracy up to 3 °C. |
| Furnace lining | Integral structure of polycrystalline mullite fibres, small volume, good insulation, low energy consumption, high efficiency, temperature above 1200 °C, long service life. |
| Operation | Simple to operate, and the power can be adjusted with the work. |
| Load duration | 100 % load duration, maximum power, ensuring 24 hours of operation. |
| Mould and casting | Precisely engineered moulds for accurate casting dimensions and consistent quality, with refractory materials that withstand molten alloy temperatures; automated control of pouring, cooling and ejection; enclosed casting areas, emergency stop systems and proper ventilation; ingots and billets for further processing into sheet, extrusions or castings. |
Recommended Model Selection
A brass furnace is selected on three things in this order: the alloy family, the batch weight, and the vessel. The published capacity tiers give the frame, and the model table gives the machine.
| Capacity tier | Capacity range | Power range | Frequency range | Primary market | Typical cycle time |
|---|---|---|---|---|---|
| Small / Laboratory | 5-100 kg | 15-75 kW | 2,000-8,000 Hz | Jewelry, R&D, art casting, small foundry | 15-45 min/heat |
| Medium / Workshop | 100-1,000 kg | 75-750 kW | 500-2,500 Hz | Brass/bronze foundry, die casting, valve production | 45-120 min/heat |
| Large / Industrial | 1,000-5,000 kg | 750-3,500 kW | 250-1,000 Hz | Copper recycling, wire rod, continuous casting, anode production | 90-240 min/heat |
Within the medium and workshop tier, HLQ publishes a specific set of models with their copper capacity, melting rate, power consumption and operating frequency, which is the right table for a brass shop choosing a furnace.
| Model | Rated capacity (copper) | Max input power | Melting rate (copper) | Power consumption | Operating frequency |
|---|---|---|---|---|---|
| MF-70 | 100 kg | 70 kW | About 110 kg/hr | About 350 kWh/ton | 1000-2000 Hz |
| MF-120 | 250 kg | 160 kW | About 240 kg/hr | About 330 kWh/ton | 500-1000 Hz |
| MF-250 | 500 kg | 250 kW | About 400 kg/hr | About 320 kWh/ton | 500-1000 Hz |
| MF-500 | 1,000 kg | 500 kW | About 800 kg/hr | About 300 kWh/ton | 200-500 Hz |
Note the trend in that table: the melting rate roughly tracks the power, while the power consumption per ton falls from about 350 to about 300 kWh/ton as the furnace gets larger. The operating frequency falls with it, from 1000-2000 Hz on the smallest to 200-500 Hz on the largest, because a deeper current penetration suits a deeper bath of dense copper alloy. On the SMJD series itself, the published brass and copper capacity by model runs 500 kg at SMJD-463 and SMJD-480, 600 kg at SMJD-580, 560 kg at SMJD-600, 900 kg at SMJD-900 and SMJD-905, 1,200 kg and 1,350 kg at the two SMJD-1250 ratings, 1,500 kg at SMJD-1500, 1,560 kg at SMJD-1550, 1,700 kg at SMJD-1700, 2,000 kg at SMJD-2300 and 3,000 kg at SMJD-3100.
For the small-batch end, HLQ publishes the DW-MF brass system separately: 15-160 kW maximum input, 1-20 kHz with typical 4, 8, 11, 15 or 20 kHz, 3 × 380 V ±20 %, 100 % duty cycle, 3-500 kg melting capacity, about 50-60 minutes from a cold furnace and 20-30 minutes in a hot one, in tilting, push-up and stationary furnace types. The full engineering reference for the industrial range is the 5000 kg copper melting induction furnace page, and the general copper smelter route is the induction copper melting furnace page.
Process Workflow
A brass melt is a controlled sequence, not a heat, and HLQ publishes a twelve-step version of it in which every step carries a stated control point. Steps 7 to 10 are the ones that distinguish brass from every other alloy on this site.
| Step | Action | Control point |
|---|---|---|
| 1 | Inspect the lining and cooling water; start fume extraction | Extraction running throughout the heat |
| 2 | Preheat the lining or crucible | Avoid thermal shock |
| 3 | Sort the charge by alloy, weigh it and pre-dry the scrap | No wet scrap in a hot furnace |
| 4 | Load dense material first | Charge order |
| 5 | Raise power gradually | Controlled ramp |
| 6 | Add the remaining charge as the first batch melts | Do not flood the bath |
| 7 | Apply a flux cover (charcoal or copper flux) | Keep the cover on during the heat |
| 8 | Add zinc as the last element | Limits zinc loss |
| 9 | Hold at 950-1,020 °C | Never above 1,050 °C; short holding |
| 10 | Skim the dross | Clean surface before pouring |
| 11 | Check the temperature and take a sample | Cu-Zn composition |
| 12 | Tilt and pour into a ladle or moulds | Controlled discharge |
Steps 1 and 3 are the ones that protect the operator and the lining: the extraction is started before the heat, not after the first fume, and no wet scrap goes into a hot furnace. Steps 7 and 8 are the ones that protect the metal: the flux cover stays on, and the zinc goes in last. Step 9 is the one that protects the specification: hold between 950 and 1,020 °C, never above 1,050 °C, and keep the holding short. Step 11 is the one that catches a problem before the customer does, because a sample is the only way to know the Cu-Zn composition of the heat.
There is one rule in this sequence that applies to the whole shop rather than to a single heat. HLQ’s published alloy switching rule is that pure copper must not be melted in a lining used for brass, because zinc absorbed in the lining can contaminate the copper. Use a dedicated lining or a dedicated furnace for each alloy family. It is also the published failure mode for a brass shop that has been running both metals on one furnace.
Common Problems and Solutions
The published troubleshooting reference for brass covers the failures a brass shop actually meets, and four of the seven are unique to a copper-zinc alloy rather than to induction melting in general.
| Problem | Likely cause | Published solution |
|---|---|---|
| Zinc fuming | Temperature above 1,050 °C; long holding | Reduce to 950-1,000 °C; minimise holding; add zinc last; check fume extraction |
| Hydrogen porosity in castings | Wet or oily scrap; damp flux | Pre-dry all scrap and flux; purge with dry argon |
| Rapid lining erosion | Wrong lining chemistry, overheating, poor sintering, thermal shock | Use a silica lining; follow the sintering protocol; preheat the charge |
| Alloy out of specification | Charge error, volatile zinc loss, contaminated scrap | Recalculate the charge; add volatile elements last; use certified scrap |
| Inconsistent chemistry between heats | Variable scrap, manual addition errors, sampling | Sort scrap; standardise sampling |
| Pure copper contaminated after brass | Zinc absorbed in the lining | Use a dedicated lining or furnace for each alloy family |
| Furnace fails to start | Coil insulation fault, water flow alarm, IGBT or capacitor fault | Check coil insulation (> 1 MΩ), water flow, IGBT and capacitor fuses |
The third row is a lining problem that presents as a furnace problem, and the last row is the routine check that keeps a brass shop running: coil insulation above 1 MΩ, water flow present, and the IGBT and capacitor fuses sound. The second row is the one that catches a workshop out: hydrogen porosity in brass castings is almost always wet scrap or damp flux, and no amount of temperature control fixes it.
Engineering Selection Guide
Selecting a brass furnace is a matter of answering eight questions in order, and HLQ publishes them as the selection factors. The order matters: the first answer decides the lining, and the lining decides the furnace.
| Selection factor | What to confirm | Published recommendation |
|---|---|---|
| Brass grade | C26000, C28000, C36000 or other | Sets the melt temperature and ventilation needs (lead in C36000) |
| Throughput | Net kg/h with a 70 % utilization factor | Sets furnace capacity and power |
| Charge form | Ingot, returns or scrap | Scrap must be sorted and dried |
| Lining | Dedicated to brass or shared with other alloys | Silica; keep a separate lining for pure copper |
| Fume extraction | Hood above the furnace | Required for zinc and lead fumes |
| Pouring | Manual, electrical or hydraulic tilt | Hydraulic for larger batches |
| Scale-up | Future capacity | The 5,000 kg copper melting induction furnace range covers brass up to industrial size |
| Alloy switching | Which alloys will share the furnace | Dedicated lining or furnace per alloy family |
Two published comparisons sharpen those answers. The first is the alloy switching rule already noted: brass takes silica, pure copper takes magnesia, and the failure mode of each is the other’s hazard, so the published recommendation is a dedicated lining or furnace per alloy family. The second is the plant layout, and it is where the fume hood and the lining store have to appear on the drawing rather than in the budget.
The published plant ranges below give the wider envelope, and the published selection factor for throughput — net kg per hour with a 70 % utilization factor — is the number that actually sizes the furnace, because a brass shop that quotes a nameplate capacity rather than a net hourly rate will be short of metal every shift.
| Parameter | Published range | Notes |
|---|---|---|
| Batch capacity | 0.5 kg (gold) to 5,000 kg | Customised to batch weight and daily output |
| Power | 3 kW (small gold melters) to 3,500 kW (large copper furnaces) | Set by batch weight and target melting time |
| Frequency | Gold about 1-80 kHz; aluminum about 0.5-20 kHz; copper about 0.25-8 kHz; iron and steel about 0.5-2.5 kHz | Lower frequency is used for larger furnaces |
| Input voltage | 380 V, 660 V, 750 V, 1,000 V or customised | Depends on power level and plant supply |
| Furnace body | Steel shell or aluminum shell | Steel shell for larger, heavy-duty furnaces |
| Tilting | Hydraulic, gearbox or manual; fixed design possible | Hydraulic tilting recommended for medium and large furnaces |
| Cooling | Closed-loop cooling tower or industrial chiller | For coil, power supply, capacitors and cables |
| Temperature measurement | Thermocouple, immersion probe or infrared pyrometer | Immersion measurement is common for molten metal |
| Control | Manual, digital, PLC or HMI | Automation improves repeatability |
| Protection | Over-current, over-voltage, water pressure, phase loss; leak alarm optional | Full protection recommended for large iron and steel furnaces |
Two published comparisons close the guide. The first is against a gas or crucible furnace, and it is the argument for induction on a brass line specifically. The second is the published operation-type power density, which is what tells a buyer whether the furnace is being sized for a fast brass melt or a scrap remelt.
| Feature | Induction copper melter | Gas / crucible furnace |
|---|---|---|
| Melting speed | Very fast. A full 500 kg batch melts in 40-60 minutes from a cold start. | Slow. Requires long preheat and extended melting cycles. |
| Metal purity | Very high. Minimal oxygen and hydrogen pickup due to rapid, flameless melting. | Lower. High risk of gas porosity and dross from combustion byproducts. |
| Metal loss (burn-off) | Extremely low (<1 %). Rapid melting drastically reduces oxidation. | High (3-5 %+). Prolonged exposure to flame causes significant metal loss. |
| Temperature control | Precise (±5 °C). Instant power control prevents overheating. | Difficult. Prone to temperature fluctuations and overheating. |
| Energy efficiency | High. Over 95 % electrical efficiency; minimal heat radiated into the workshop. | Low. Massive heat loss through exhaust flue and radiation. |
| Environment and safety | Clean and safe. No CO2, no fumes, no open flame, and a cooler working area. | Polluting and hazardous. Emits CO2/NOx; high fire risk and ambient heat. |
| Footprint | Compact. Requires significantly less floor space. | Bulky. Needs space for the furnace, fuel storage, and flue systems. |
| Operation type | Recommended power density (kW/t) | Published note |
|---|---|---|
| Rapid batch melting (ingot charge) | 450-600 kW/t | Maximum melting speed; shortest cycle time |
| Standard batch melting (mixed charge) | 350-450 kW/t | Balanced speed and energy efficiency |
| Scrap remelting (variable density) | 300-400 kW/t | Lower density scrap; longer effective cycle |
| Holding and temperature maintenance | 100-200 kW/t | Compensating for heat losses only |
| Continuous casting (melting + holding) | 250-350 kW/t | Steady-state supply to casting machine |
On a brass line the scrap row is the one to read carefully: sorted brass returns carry a bulk density of 2-5 kg/dm³ against 8.4-8.5 kg/dm³ for solid metal, so a scrap duty sits in the lower power-density band and runs a longer effective cycle. A furnace specified on the ingot-charge band and fed with returns will run behind all day, and the published scrap-remelting band is the number to specify against.
Advantages and Limitations
Advantages
| Potential advantage | Engineering explanation | Condition / qualification |
|---|---|---|
| Electromagnetic stirring distributes zinc evenly | The rotating field mixes the melt, so the zinc does not stratify through the bath. | Improves castings; it does not replace the temperature window. |
| Precise power control holds the melt window | Closed-loop power control holds 950-1,020 °C. | The window must be held to limit zinc loss; it is not automatic without the recipe. |
| Stirring helps flux and oxides float | The flux cover and the field together lift oxide out of the melt. | Cleaner castings, but the cover still has to be applied and kept on. |
| Fast cycle on a hot furnace | Published about 20-30 minutes per melt in a hot furnace. | About 50-60 minutes from a cold furnace on the DW-MF system. |
| One furnace, many alloys | Published as able to melt copper, bronze, silver, gold and aluminum. | Only with a separate lining and crucible per alloy family. |
| Very low metal loss against a gas furnace | Published metal loss under 1 % against 3-5 % or more for a gas or crucible furnace, because there is no flame in contact with the melt. | The comparison is against the published gas furnace figures; on a brass line it protects the Cu-Zn composition as well as the yield. |
| Precise temperature control | Published ±5 °C control with instant power response. | Prevents the overheating that drives zinc loss. |
| Clean, cool workshop | No CO2, no combustion fumes from the heating method, and minimal radiated heat. | Fume extraction is still required for the zinc and lead the charge itself carries. |
Limitations
| Limitation | Consequence | Better approach |
|---|---|---|
| Zinc fuming needs dedicated extraction | Zinc and lead fumes are produced by the charge itself, so an induction furnace does not solve the ventilation problem. | Run fume extraction throughout the heat with a hood over the furnace; treat the extraction as production-critical. |
| The temperature window must be held | The published window is 950-1,020 °C and never above 1,050 °C. Above it, zinc leaves the melt. | Hold the window, keep holding time short, add zinc last, and check the temperature at the published sample step. |
| Alloy contamination between linings | A lining used for brass will contaminate pure copper with absorbed zinc, and the failure is discovered on the customer’s casting rather than in the furnace. | Use a dedicated lining or furnace for each alloy family, and keep the linings stored and identified separately. |
| Lead-bearing grades need ventilation | C36000 free-cutting brass carries lead, which is a workplace issue as well as a process one. | Ventilation required for the grade, and a decision on whether that grade belongs on the same line as the rest. |
| Cooling water is required | The coil, power supply, capacitors and cables all generate heat; insufficient cooling causes alarms, insulation damage, coil failure or safety hazards. | Use a closed-loop cooling tower or industrial chiller with flow and pressure protection. |
| Scrap is a lower-density, longer-cycle duty | Sorted returns carry a bulk density of 2-5 kg/dm³, so the melt takes longer and produces more dross. | Size against the published scrap remelting band of 300-400 kW/t rather than the ingot band, and budget for the dross stream. |
| Molten-metal hazards remain | Burn, splash, fume and moisture-contact risks are not removed by induction heating. | Use a controlled workspace, PPE, extraction and trained operators. |
Why Choose HLQ?
HLQ Induction Equipment has been developing and producing high frequency and medium frequency induction heating and melting equipment for 25 years, and the published copper-alloy material is the most complete on the site: three SMJD specification tables including the crucible drawing, a manufacturer manual with the heating principle and the commercial terms, and a set of alloy, lining and troubleshooting references that a foundry can actually specify against.
| Published item | Detail |
|---|---|
| Warranty | 12 months from the contract signed date. |
| Test machine running | HLQ’s technical staff test the machine running before shipment; all machines are tested and debugged carefully before shipment. |
| Quality control | Professional QC personnel inspect machinery during production; the QC team complies with TQM, with each step in compliance to the standards. Photos and video can be provided on request. |
| Delivery | If the buyer has shippers in China the machine can be sent to them free of charge; otherwise it can be sent directly to any main port of China promptly. |
| Packaging | Wrapped with a film layer for waterproof, packed in a paper box, then put into a wooden case (standard exporting carton) and wrapped with foam around for shockproof. |
| Storage conditions | Clean, dry environment; temperature -20 to 60 °C; humidity 0-95 % with no dew; avoid corrosive gases and liquids. |
| After-sales service | Engineers are sent to the customer’s workshop, with installation, debugging and training until the machine is in normal production. |
| Published services | Immediate reply to your inquiry; detailed product and company information; best quotation; immediate reply to your questions; technical support or alternative accessories if necessary. |
| Product range | IGBT medium frequency induction heating equipment, IGBT super audio induction heating equipment, CNC quenching machine tool, IGBT medium frequency induction melting furnace, KGPS medium frequency induction melting furnace, open type water cooling tower and closed water cooling tower. |
For a brass buyer the three items that matter most are the test-running commitment, because a furnace that has not been run on a representative brass charge before shipment is a furnace whose zinc loss and dross rate are still theoretical; the engineer commissioning, because the published twelve-step sequence is only reproducible if somebody sets the recipe and the flux cover; and the twelve-month warranty, which is the only published commitment on the equipment itself.
The neighbouring HLQ pages cover the same equipment family for the other copper-alloy duties, including the copper scrap melting furnace for the scrap route, the induction aluminium melting furnace and the aluminum melting furnace for the aluminium side of the plant, the portable gold melting furnace for benchtop precious-metal work, and the magnetic induction aluminum melting furnace for the 300 kg and 500 kg class.
6 Core FAQs
1. What is an induction brass melting furnace?
It is a medium frequency electric batch furnace that melts brass, bronze and copper alloys by generating the heat inside the metal itself, with no flame in contact with the melt. The SMJD series covers thirteen sizes from SMJD-463 to SMJD-3100, with a published copper, gold and silver capacity of 500 kg per heat at SMJD-463 rising to 3,000 kg at SMJD-3100, from 60 kW to 200 kW input, published input current 90 A to 300 A, a 3-phase 380 V 50-60 Hz supply, oscillation frequency from 1 kHz to 100 kHz with a custom frequency on request, and a maximum furnace temperature of 1800 °C. The power devices are IGBT, with automatic load impedance matching, closed-loop power control, PID heating control and an LED digital controller accurate to 3 °C, and a published 100 % load duration for 24 hours. Note that the published capacity table’s middle column is the copper and precious-metals one; neither brass nor bronze is named in its heading, so the brass figure for a quotation is taken from that second column and confirmed against the alloy data.
2. Why is brass harder to melt than aluminum, and what controls it?
Because the alloy contains zinc and zinc is volatile. HLQ publishes brass melting at about 885-955 °C depending on grade, and zinc boiling at 907 °C, so zinc loss is the main process risk. The published controls are four: hold the melt at 950-1,020 °C and never above 1,050 °C; keep the holding time short; add zinc as the last element; and keep a flux cover on the melt, charcoal or copper flux, throughout the heat. Fume extraction runs the whole time, because the zinc and lead fumes come from the charge itself and induction heating does not remove them.
3. Which lining should a brass furnace have, and can the same furnace melt copper?
Brass takes an acidic silica lining, published at SiO₂ ≥ 97 %, sintered at 1,050-1,100 °C with an expected life of 200-400 heats and thermal cycling erosion as the primary failure mode. Pure copper takes a basic magnesia lining at MgO ≥ 90 %, because the published failure mode for copper on silica is Cu₂O chemical attack. The two are each other’s hazard, and the published rule is that pure copper must not be melted in a lining used for brass, because zinc absorbed in the lining can contaminate the copper. Use a dedicated lining or a dedicated furnace for each alloy family, and store and identify the linings separately.
4. How long does a brass heat take, and how much does it cost to melt?
On the published DW-MF brass system, about 50-60 minutes from a cold furnace and 20-30 minutes in a hot one, at 15-160 kW maximum input and 3-500 kg melting capacity. On the published model tables, a 100 kg copper batch melts at about 110 kg per hour for about 350 kWh per ton on MF-70, and a 1,000 kg batch at about 800 kg per hour for about 300 kWh per ton on MF-500, so the larger furnace is both faster and cheaper per ton. Against a gas or crucible furnace the published comparison is very large metal loss under 1 % against 3-5 % or more, and precise temperature control at ±5 °C against fluctuating gas furnace temperatures.
5. Can the same furnace melt brass, bronze and copper, and what about scrap?
Yes, and the published application for laboratory and small casting is explicitly flexible alloy switching, provided each alloy family gets its own lining and crucible. Scrap is a different duty: the published note for brass returns and scrap is to sort by alloy, pre-dry and manage dross, and the published bulk density for returns is 2-5 kg/dm³ against 8.39-8.53 kg/dm³ for solid brass, so a scrap heat is roughly a quarter of the density and needs the published scrap remelting power band of 300-400 kW/t rather than the rapid ingot band of 450-600 kW/t. For brass scrap the published route also includes zinc recovery by vacuum distillation, which is a separate piece of equipment.
6. What should I confirm with the supplier before ordering?
Eight things, in this order. The brass grade, because it sets the melt temperature and the ventilation requirement and, for C36000, the lead content. The net throughput in kg per hour with a 70 % utilization factor, because that is what sizes the furnace and the power rather than the nameplate capacity. The charge form, since scrap must be sorted and dried. The lining arrangement, with a dedicated lining for brass and a separate one for pure copper. The fume extraction, running throughout the heat. The pouring method, manual, electrical or hydraulic tilt, with hydraulic recommended for larger batches. The future scale-up, because the 5,000 kg copper melting range covers brass up to industrial size. And the acceptance criterion in writing, for example 500 kg of a specified brass grade from ambient to pour-ready in a stated number of minutes, with a Cu-Zn sample and an alloy analysis, backed by a representative melt-test record before shipment.