Induction Brazing Short-Circuit End Rings on Copper Rotors
Induction Brazing Short-Circuit End Rings on Copper Rotors: Process, Equipment and Selection Guide
A short-circuit ring (SCR) is brazed to the rotor of an electrical motor, particularly in the squirrel cage type, where the name for the rotor and for the motor itself comes from the same construction. The temperature homogeneity in the ring is absolutely critical to meet the technical requirements of the finished motor or generator, so control of the process and brazing experience in this field are requirements rather than options.
Induction heating offers several advantages over traditional flame methods for brazing short-circuit rings. One key advantage is that induction generates a more homogeneous temperature distribution around the SCR. Because induction heating can be controlled precisely, overheating of the copper bars is avoided. Induction heating is also fast: its accuracy and repeatability mean throughput can be increased without sacrificing joint quality.
This guide covers the full application for medium to high power motors and generators, including the two brazing routes, the machine range, the temperature control strategy, the process workflow and the engineering selection criteria for a new line or a retrofit.

Quick Answer
Induction brazing of a short-circuit end ring works by heating the copper ring itself with an electromagnetic field until the brazing filler alloy melts and is drawn into the clearance between the ring and the rotor bars by capillary action. The base metal is heated first, and the filler, which has the lower melting range, is the part that flows, so the copper itself is never taken to a damaging temperature.
There are two ways to braze an SCR. Single shot brazing applies one power application to heat the whole ring at once and needs more heating power. Segment brazing heats and brazes the ring in overlapping segments with the rotor indexed between passes. The major difference between the two methods is power demand: when the diameter of the SCR is less than 1200 mm, single shot brazing is used.
HLQ Induction Equipment’s series power generators provide a wide range of heating power from 25 kW up to 200/320 kW for this work. A temperature regulating system can be integrated into an infrared temperature controller for closed loop control of the brazing power. Normally there are two controlled pyrometers in the system: one for measuring the temperature in the SCR and the other for measuring the temperature on the copper bar to ensure it reaches the brazing temperature.
For the wider machine range, see the induction brazing machine category, and for the medium frequency series that carries most rotor work, see the medium frequency series of power generators.
Table of Contents
- What is the SCR Induction Brazing Machine?
- Key Applications
- Suitable Materials
- Working Principle
- Technical Specifications
- Recommended Model Selection
- Process Workflow
- Common Problems and Solutions
- Engineering Selection Guide
- Advantages and Limitations
- Why Choose HLQ?
- 6 Core FAQs
What is the SCR Induction Brazing Machine?
An SCR induction brazing machine is an electromagnetic heating system that makes a brazed joint between a copper short-circuit ring and the rotor bars of a conductive rotor. The ring and bars are cleaned, fluxed and fitted with a brazing filler alloy. An induction coil is placed around the ring, and current in the coil induces current in the copper parts themselves. The parts heat, the filler melts, and the molten filler flows into the joint clearance by capillary action. When the joint cools it is metallurgically continuous, not a mechanical fit and not a welded seam.
The machine itself is simpler than the process. A power supply cabinet converts mains electricity into a controlled frequency output. A remote workhead carries the capacitor bank and the output coupling close to the work. A coil, solid, split, or flexible, is placed around or beside the joint. The control section sets the power, the heating time and the cooling time. The timer model allows the power, the operating time of the heating period and the cooling period to be preset respectively, to realise a simple heating curve, and this model is suggested for batch production to improve repeatability. Separated models are designed to fit the dirty surroundings of some cases.
What distinguishes an SCR line from a general-purpose induction brazing station is the coil. HLQ’s coil design, together with induction heating’s speed and accuracy, means minimal heat input. This in turn reduces the risk of shafts weakening, and minimizes heat transfer into the laminations, which is a common problem when using flame brazing. A dedicated induction heating coil is therefore specified for the ring, and coil selection is discussed in the selection guide below.

Key Applications
Published induction brazing applications fall into two families: joining metal parts with a filler alloy, and heating metal parts to a temperature for another purpose. Motor component brazing is the published category that covers rotor work, and the table below sets out what each published application needs.
| Published application | Materials | Published recommended power | Published frequency |
|---|---|---|---|
| Motor component brazing | Copper bars, terminals | 30–120 kW | 20–100 kHz |
| Small copper tube brazing | Copper to copper, copper to brass | 5–15 kW | 80–300 kHz |
| HVAC distributor brazing | Copper tubes and brass fittings | 15–35 kW | 50–200 kHz |
| Medium copper pipe joint | Copper, brass | 25–60 kW | 30–150 kHz |
| Stainless steel tube brazing | Stainless steel, copper, nickel alloy | 15–50 kW | 50–200 kHz |
| Carbide tool brazing | Carbide to steel | 15–80 kW | 20–100 kHz |
| Diamond segment brazing | Diamond segment to steel body | 25–100 kW | 20–100 kHz |
| Electrical connector brazing | Copper, brass, silver alloy | 10–40 kW | 80–300 kHz |
| Cookware bottom brazing | Stainless steel, aluminium, copper plate | 80–250 kW | 10–50 kHz |
| Automatic multi-station brazing | Various metal assemblies | 50–300 kW | 10–200 kHz |
For a squirrel cage rotor the job is a large, heavy copper-to-copper joint distributed around a full circumference, which places it well above the tube and connector duties in both mass and required temperature uniformity. The published benefit list for this application includes less part distortion and less joint stress than welding, and finished brazed copper joints are identical because the machine repeats the same power and time setting on each one.
Related rotor-side operations use the same machine family and the same thermal control philosophy. These include rotor shaft shrink fitting, housing shrink fitting, and stator copper strip brazing, all of which appear as companion technologies to the SCR brazing application. For the general principles behind the heating itself, see the induction brazing jointing equipment application page.
Suitable Materials
The base material decides the filler, the temperature window and how hard the job is. The published assessment is reproduced below.
| Base material | Brazing suitability | Common filler metals | Engineering note |
|---|---|---|---|
| Copper | Excellent | Silver alloy, copper-phosphorus alloy | High thermal conductivity requires enough power and good coil coupling |
| Brass | Excellent | Silver alloy, brass brazing alloy | Control temperature to avoid zinc evaporation and discoloration |
| Carbon steel | Excellent | Silver alloy, copper alloy, nickel alloy | Magnetic material heats efficiently at lower frequency |
| Stainless steel | Good | Silver alloy, nickel alloy | Often benefits from flux or a protective atmosphere |
| Carbide | Good | Silver-copper alloy | Requires controlled heating to reduce thermal stress and cracking |
| Diamond tool segments | Good | Silver-based brazing alloy | Temperature control is critical to protect diamond performance |
| Aluminium | Possible but more difficult | Aluminium brazing alloy | Narrow temperature window and oxide film control are important |
| Copper to steel | Good | Silver alloy, copper alloy | Different heating rates require coil and fixture balancing |
| Copper to brass | Excellent | Silver alloy, copper-phosphorus alloy | Common in HVAC and plumbing components |
For the rotor end ring the joint is copper ring to copper bar, which sits in the best category in this table. The engineering note on copper is the one that governs the whole machine selection: high thermal conductivity requires enough power and good coil coupling. Copper also means the heat leaves the joint quickly along the bar and the ring, so a tight, uniform coil coupling is what makes the temperature homogeneous around the circumference.
The material properties that decide frequency and power are set out below, as published for the medium frequency generator range.
| Material property | Effect on induction heating |
|---|---|
| Electrical resistivity | Influences induced current distribution and heating |
| Magnetic permeability | Strongly influences penetration in ferromagnetic materials |
| Thermal conductivity | Influences temperature equalization |
| Specific heat capacity | Determines sensible heating energy |
| Workpiece diameter | Influences frequency and heating-time selection |
| Phase transformation | May change thermal and magnetic properties |
| Target temperature | Determines required thermal energy |
The heating characteristics of the candidate ring and bar materials complete the picture.
| Material | Heating characteristics | Typical application | Engineering consideration |
|---|---|---|---|
| Carbon steel | Ferromagnetic below Curie temperature | Forging and heat treatment | Magnetic properties change during heating |
| Alloy steel | Grade-dependent magnetic and thermal properties | Forging and hardening | Metallurgical temperature limits |
| Stainless steel | Depends on stainless steel grade | Heating and heat treatment | Magnetic and non-magnetic grades behave differently |
| Copper | High electrical and thermal conductivity | Billet heating and melting | Coil coupling and heating efficiency |
| Brass | Nonferrous copper alloy | Forging and melting | Alloy composition and temperature |
| Bronze | Properties depend on alloy | Forging and melting | Alloy-specific process requirements |
| Aluminum | High thermal conductivity | Billet heating and melting | Coil design and temperature distribution |
| Cast iron | Grade-dependent | Melting and heating | Melting and heating temperature requirements |
Working Principle
The published process runs in six stages, and the control point of each stage is what makes the joint repeat rather than merely get hot.

| Stage | Physical action | Engineering control point |
|---|---|---|
| 1. Power conversion | AC input is converted into high-frequency output | Power, frequency, duty cycle and inverter stability |
| 2. Magnetic field generation | Current flows through the induction coil | Coil turns, coil diameter, copper tube size and cooling |
| 3. Workpiece heating | Eddy currents generate heat in the joint area | Coupling distance, heating depth and part position |
| 4. Filler melting | Brazing alloy melts before the base metal | Temperature window and heating uniformity |
| 5. Capillary flow | Molten filler flows into the joint gap | Joint clearance, surface cleanliness and flux |
| 6. Cooling and solidification | The joint becomes mechanically strong | Cooling speed, fixture holding time and oxidation control |
Two features of stage 4 decide the whole result. The filler alloy has a lower melting range than the base metals, so a correctly controlled joint reaches the point where the filler flows before the copper, brass or steel is damaged. And because the heating is localised to the coil, the rest of the part stays cool, which is why a brazed copper joint can be handled straight after the cycle.
The joint is the only hot zone. The copper of the ring and the bars is heated by the induced current, and the filler flows in the gap between them. The coil is placed around the ring so that the entire circumference is inside the field at the same time, which is what produces the homogeneous temperature distribution that this application depends on.
Control is closed loop. A temperature regulating system can be integrated into an infrared temperature controller for closed loop control of the brazing power, and there are normally two controlled pyrometers: one measuring the temperature in the SCR and one measuring the temperature on the copper bar. The second pyrometer matters because the bar and the ring do not heat at the same rate, and the joint is only made when both have reached the brazing temperature.
Technical Specifications
The published catalogue data for the medium frequency series, which is the band used for rotor-scale work, is reproduced below exactly as published, with the spelling errors cleaned up.
| Model | Input power max | Input current max | Oscillation frequency | Input voltage | Duty cycle |
|---|---|---|---|---|---|
| DW-MF-15 Induction Generator | 15 kW | 23 A | 1–20 kHz | 3 phases, 380 V ±10 % | 100 % |
| DW-MF-25 Induction Generator | 25 kW | 36 A | 1–20 kHz | 3 phases, 380 V ±10 % | 100 % |
| DW-MF-35 Induction Generator | 35 kW | 51 A | 1–20 kHz | 3 phases, 380 V ±10 % | 100 % |
| DW-MF-45 Induction Generator | 45 kW | 68 A | 1–20 kHz | 3 phases, 380 V ±10 % | 100 % |
| DW-MF-70 Induction Generator | 70 kW | 105 A | 1–20 kHz | 3 phases, 380 V ±10 % | 100 % |
| DW-MF-90 Induction Generator | 90 kW | 135 A | 1–20 kHz | 3 phases, 380 V ±10 % | 100 % |
| DW-MF-110 Induction Generator | 110 kW | 170 A | 1–20 kHz | 3 phases, 380 V ±10 % | 100 % |
| DW-MF-160 Induction Generator | 160 kW | 240 A | 1–20 kHz | 3 phases, 380 V ±10 % | 100 % |
Published note on the MF series: the input voltage is stated as “according to the application”, with 3 phases 380 V ±10 % as the standard configuration.
For larger rotors, the published MFS series of medium frequency heating systems covers the higher power band.
| Model | Rated output power | Frequency range | Input current | Water flow | Weight | Dimension |
|---|---|---|---|---|---|---|
| MFS-100 | 100 kW | 0.5–10 kHz | 160 A | 10–20 m³/h | 175 kg | 800×650×1800 mm |
| MFS-160 | 160 kW | 0.5–10 kHz | 250 A | 10–20 m³/h | 180 kg | 800×650×1800 mm |
| MFS-200 | 200 kW | 0.5–10 kHz | 310 A | 10–20 m³/h | 180 kg | 800×650×1800 mm |
| MFS-250 | 250 kW | 0.5–10 kHz | 380 A | 10–20 m³/h | 192 kg | 800×650×1800 mm |
| MFS-300 | 300 kW | 0.5–8 kHz | 460 A | 25–35 m³/h | 198 kg | 800×650×1800 mm |
| MFS-400 | 400 kW | 0.5–8 kHz | 610 A | 25–35 m³/h | 225 kg | 800×650×1800 mm |
| MFS-500 | 500 kW | 0.5–8 kHz | 760 A | 25–35 m³/h | 350 kg | 1500×800×2000 mm |
| MFS-600 | 600 kW | 0.5–8 kHz | 920 A | 25–35 m³/h | 360 kg | 1500×800×2000 mm |
| MFS-750 | 750 kW | 0.5–6 kHz | 1150 A | 50–60 m³/h | 380 kg | 1500×800×2000 mm |
| MFS-800 | 800 kW | 0.5–6 kHz | 1300 A | 50–60 m³/h | 390 kg | 1500×800×2000 mm |
The published MFS input voltage is 3 phase 380 V 50 Hz with a 100 % duty cycle. The DW-MF-160KW model specification is given below as published.
| Product information | Specification |
|---|---|
| Manufacturer | HLQ Induction Equipment Co., Ltd. |
| Product | Medium Frequency Induction Generator |
| Model | DW-MF-160KW |
| Maximum oscillation power | 160 kW |
| Operating frequency | 1–20 kHz |
| Electrical supply | Three-phase AC 380 V |
| Inverter technology | IGBT parallel inverter |
| Cooling | Water cooling |
| Primary applications | Forging, metal heating and melting |
| Operating duty | Published 100 % duty cycle at 40 °C |
The full published specification of the medium frequency induction power generator covers the protection and installation details that matter for a cell installation.
| Technical parameter | Specification |
|---|---|
| Product name | Medium Frequency Induction Power Generator |
| Product category | Medium Frequency Induction Heating Power Supply |
| Manufacturer | HLQ Induction Equipment Co., Ltd. |
| Brand | HLQ |
| Model number | DW-MF-15KW |
| Maximum oscillation power | 15 kW |
| Operating frequency | 1–20 kHz |
| Input voltage | Three-phase AC 380 V |
| Input frequency | 50/60 Hz |
| Published maximum input current | 23 A |
| Power electronics | IGBT inverter |
| Inverter circuit | Parallel inverter configuration |
| Heating principle | Electromagnetic induction |
| Cooling method | Water cooling |
| Required cooling water pressure | > 0.2 MPa |
| Published cooling water flow | 6 L/min |
| Duty cycle | 100 % at 40 °C, under specified conditions |
| Generator dimensions | 560 × 270 × 470 mm |
| Transformer dimensions | 550 × 300 × 420 mm |
| Generator net weight | Approximately 30 kg |
| Transformer net weight | Approximately 35 kg |
| Cable length | 2 m |
| Induction coil | Customized according to application |
| Electrical protection | Overvoltage, overcurrent, phase-loss protection |
| Thermal protection | Overtemperature protection |
Recommended Model Selection
The model choice follows from the ring diameter, the ring mass and the choice between single shot and segment brazing. The published model-series data for the medium frequency range is reproduced below.
| Model | Rated power | Published model-series frequency | Typical application |
|---|---|---|---|
| DW-MF-15 | 15 kW | 1–20 kHz | Small rod heating, localized forging |
| DW-MF-25 | 25 kW | 1–20 kHz | Small bar heating, preheating |
| DW-MF-35 | 35 kW | 1–20 kHz | Steel rod heating |
| DW-MF-45 | 45 kW | 1–20 kHz | Billet end heating |
| DW-MF-70 | 70 kW | 1–20 kHz | Forging and bar heating |
| DW-MF-90 | 90 kW | 1–20 kHz | Industrial forging |
| DW-MF-110 | 110 kW | 1–20 kHz | Medium-duty heating |
| DW-MF-160 | 160 kW | 1–20 kHz | Larger billet heating |
| DW-MF-300 | 300 kW | 1–20 kHz | Heavy-duty industrial heating |
The published selection logic for this family is set out below, expressed in the terms that apply to rotor work.
| Selection factor | What it decides on an SCR job |
|---|---|
| Ring diameter | Sets single shot versus segment brazing. Published rule of thumb: single shot below 1200 mm diameter |
| Ring and bar mass | Determines the sensible heating energy needed per cycle |
| Electrical conductivity of the copper | Sets coupling efficiency and therefore the power margin required |
| Coil geometry | Segmented coil selected for temperature uniformity across the full circumference |
| Line throughput | Determines whether a single station or a multi-station arrangement is required |
| Cooling water availability | Sets the required water flow and the cooling circuit specification |
| Cell environment | Determines whether a separated workhead model is needed for dirty surroundings |
| Traceability requirement | Determines the data logging and temperature curve control configuration |
The published generator range for this application provides a wide range of heating power from 25 kW up to 200/320 kW, which covers the single shot route on rings below the 1200 mm threshold and the segment route above it. For a specific machine proposal, the medium frequency induction power generator page carries the full configuration detail, and custom cell design is handled under custom induction heating applications.
Process Workflow

The published process runs in the following eight controlled stages. Stages 4 to 6 are where the temperature homogeneity of the ring is decided.
- Rotor preparation. The cage is cleaned and the bars and ring seats are free of oxide, oil and old flux residue.
- Filler and flux. The filler alloy is positioned in the joint and flux is applied to the faces to be joined.
- Coil and fixture set. The segmented coil is centred on the ring and the fixture holds the rotor square and still.
- Preheat ramp. Power is raised gradually until the pyrometers report a rising joint temperature.
- Filler melt. The filler alloy melts first and wets the copper, well below the copper melting point.
- Capillary flow. Molten filler is drawn into the clearance between the ring and the bar.
- Controlled cooling. The cooling period is preset on the controller to limit distortion and grain growth.
- Inspection. The joint is checked, ring roundness confirmed, and the rotor rebalanced only if required.
The workcell arrangement that supports those stages is set out in the layout diagram below.

The two brazing routes are compared in the diagram below.

One power application heats the whole ring at once and needs more heating power. The published rule of thumb is that single shot brazing is used when the diameter of the SCR is less than 1200 mm. When the ring is too large to reach the required temperature in one shot, the ring is heated and brazed in overlapping segments with the rotor indexed between passes, which lowers the power required per pass.
Common Problems and Solutions
The published benefits list for induction brazing of short-circuit rings identifies the specific failure modes that this process avoids, and those same failure modes are the ones that appear in production when the process is not controlled. The table below pairs each one with the control that answers it.
| Problem | Cause | Solution |
|---|---|---|
| Non-uniform ring temperature | Uneven coil coupling around the circumference | A specialized coil for extreme temperature uniformity all over the ring, combined with closed loop power control from the ring pyrometer |
| Overheating of the copper bars | Open flame or uncontrolled power applied to the whole part | Precise power control with a second pyrometer on the copper bar to confirm it reaches the brazing temperature |
| Ovality and rotor imbalance | Localized overheating and uneven thermal expansion | Minimal heat input from the induction process reduces distortion, so squirrel cage motors generally do not need rebalancing after brazing |
| Reduced shaft strength | Heat transferred into the shaft and laminations | Localized heating limits heat transfer into the laminations and reduces the risk of shafts weakening |
| Oxide film at the joint | Flux overheated by an open flame, compromising its capability to prevent oxides | Low oxide formation with no flame in the process, and a controlled heating curve that keeps the flux in its working range |
| Unwanted grain growth in the copper | Copper overheating above the brazing temperature | Precisely controlled temperature, with the filler melting before the base metal and cooling by ramps |
| Poor repeatability between rotors | Operator skill and torch technique variation | Operator expertise and brazing skills are not too critical, and the heating curve is preset on the controller for every cycle |
| Dust and fume handling burden | Open flame process in the cell | No dedusting required, no flame or gas, and easy fume removal |
Engineering Selection Guide
Use the following sequence to specify an SCR brazing cell.
- Establish the ring diameter. Below 1200 mm, plan single shot brazing and size the generator for the whole ring. Above 1200 mm, plan segment brazing and size the generator for the heated segment, with indexing between passes.
- Confirm the joint material. Copper ring to copper bar is in the excellent suitability category. Select the filler and the flux on that basis, keeping the copper-phosphorus and silver alloy families in view for the copper-to-copper case.
- Choose the frequency band. Copper is a non-ferrous, high-conductivity material, so the heating is surface-concentrated and the frequency must be matched to the coil and the ring. The published motor component brazing application sits at 30–120 kW and 20–100 kHz; the medium frequency series at 1–20 kW with greater penetration suits the heavier rotor sections.
- Check the power margin against ring mass. Higher thermal conductivity means the heat leaves the joint quickly, so enough power and good coil coupling are required to bring the ring to brazing temperature within the cycle time.
- Design the coil for uniformity, not for power. The specialized coil for extreme temperature uniformity all over the ring is the part that delivers the homogeneity the application requires.
- Specify the control system. Advanced temperature control, either a fully automated process or one managed by the brazer, using the infrared temperature controller with two controlled pyrometers, one on the SCR and one on the copper bar.
- Plan the cooling and the fixture. Preset the cooling period to control distortion and grain growth, and design the fixture to hold the rotor square and still.
- Confirm the cell services. Three-phase supply, water cooling with the published flow for the chosen model, and fume extraction. For the mid and large power range, the MFS series gives the published water flow and cabinet dimensions to plan the plant room.
- Verify the documentation requirement. If the application needs traceability for the motor’s quality records, specify the advanced control configuration and the data capture that supports repeatability and traceability.
The published frequency considerations for the medium frequency generator range are set out below, and they apply directly to the choice between the single shot and segment routes.
| Frequency consideration | Heating characteristic | Engineering implication |
|---|---|---|
| Lower frequency | Greater electromagnetic penetration | May benefit larger metal cross-sections |
| Higher frequency | More surface-concentrated current | May benefit smaller or localized heating zones |
| Workpiece diameter | Changes required heating distribution | Coil and frequency must be matched |
| Steel above Curie temperature | Magnetic permeability changes | Heating characteristics change during the cycle |
| Nonferrous materials | Different electrical and thermal properties | May require different coil matching |
| Actual operating frequency | Determined by resonant circuit and load | Cannot be selected independently of the equipment |
Advantages and Limitations
Advantages over alternative processes, as published for this application:
- Controlled process: homogenization of the heating and temperature control all around the ring.
- Fast process with higher power density, about 10 times less than flame.
- Heating by ramps totally controlled and warranted, or even cooling by ramps.
- Repeatability and traceability.
Simplified process:
- No dedusting required.
- Less distortions, no rebalance required.
- Low oxide formation.
- Operator expertise and brazing skills are not too critical.
- Running costs lower than torch.
- Eco and user-friendly operation.
Safer process:
- No flame or gas, minimized risks.
- Clear view of the process by the operator at any moment.
- Environmentally friendly.
- Easy to remove fumes.
Limitations and engineering constraints to plan for:
- Single shot brazing needs more heating power than segment brazing, so the largest ring in a given diameter band drives the power requirement.
- The ring is conductive, so heating is surface-concentrated; matching the coil to the ring diameter is essential, and the actual operating frequency is determined by the resonant circuit and load rather than selected independently of the equipment.
- The application sits in the medium to high power motor and generator segment. Below that segment, the published machine range and the process conditions change, so the published figure of about 10 times faster than flame applies to this class of work.
- Coil design and fixture design are application-specific. The published coil is customized per application, so the coil is part of the engineered solution rather than an off-the-shelf accessory.
- Closed loop control needs the pyrometer sight lines to the ring and the bar to remain clear and unobstructed as the rotor indexes between passes.
Why Choose HLQ?
HLQ Induction Equipment Co. provides solutions covering either medium to high power motors and generators, with more than 20 years of experience around the world. This application forms part of a wider portfolio for the industry.
HLQ Induction can provide customized, turn-key solutions for virtually any SCR brazing task. These solutions include the equipment, optimized temperature curves, customized coils and a comprehensive range of training and service support. The dedicated induction brazing solution for short-circuit ring work is built on three things: a specialized coil for extreme temperature uniformity all over the ring, and advanced temperature control either a fully automated process or one managed by the brazer.
The machine platform behind those solutions is documented in full, from the published power generator catalogue across the medium frequency, high frequency and ultra high frequency bands to the complete specification tables and the working published brazing cases. The induction heating PDF carries the same catalogue data in a downloadable format, and the wider equipment range is listed on the induction heating machine manufacturer page.
6 Core FAQs
1. What is a short-circuit ring and why is it brazed?
A short-circuit ring is brazed to the rotors of electric motors, particularly in the motors called “squirrel cage”, the name used for the rotor and the whole motor itself. The ring closes the electrical circuit through the rotor bars. Because the ring carries current and the finished motor must run at speed and in balance, the temperature homogeneity in the ring is absolutely critical to meet the technical requirements in the final motor or generator.
2. What is the difference between single shot and segment SCR brazing?
Induction brazing of short-circuit rings can be done in two ways: single shot and segment brazing. The major difference between the two methods is that single shot needs more heating power, because the whole ring is heated in one power application. Segment brazing heats and brazes the ring in overlapping segments with the rotor indexed between passes, which lowers the power needed per pass. When the diameter of the SCR is less than 1200 mm, single shot brazing is used; larger rings are handled by segment brazing.
3. Why does induction beat flame for brazing a rotor end ring?
Three effects decide it. Induction generates a more homogeneous temperature distribution around the SCR, which is the property the finished motor depends on. Induction heating can be controlled precisely, so overheating of the copper bars is avoided. And induction heating is fast: its accuracy and repeatability means throughput can be boosted without sacrificing quality. The published process runs about 10 times faster than flame, with low oxide formation, less distortion, no rebalancing needed and no open flame or gas in the cell.
4. What temperature control is used for an SCR brazing cell?
A temperature regulating system can be integrated into an infrared temperature controller for closed loop control of the brazing power. Normally there are two controlled pyrometers in the system: one for measuring the temperature in the SCR and the other for measuring the temperature on the copper bar to ensure it reaches the brazing temperature. Heating is applied by ramps and cooling can also be controlled by ramps, which supports repeatability and traceability on every rotor.
5. How much power is needed to braze a rotor end ring?
HLQ Induction Equipment’s series power generators provide a wide range of heating power from 25 kW up to 200/320 kW for this application. The published motor component brazing application, which covers copper bars and terminals, recommends 30–120 kW at 20–100 kHz. Within the medium frequency series, the DW-MF-15 to DW-MF-160 generators run at 1–20 kHz and the DW-MF-300 at 300 kW, while the MFS systems extend from 100 kW to 800 kW for the largest rotors. The final figure depends on the ring diameter, the ring mass and whether single shot or segment brazing is used.
6. What problems does induction brazing avoid on a squirrel cage rotor?
It avoids the four failures that flame causes on this joint. Minimal heat input reduces the risk of shafts weakening and minimizes heat transfer into the laminations. Precise temperature control reduces the risk of ovality and the subsequent need to re-balance squirrel cage motors. The flux is not overheated in an open flame, so its capability to prevent oxide formation in the joint is not compromised, and the copper is not overheated, which avoids unwanted grain growth. There is also no dust to remove and no flame or gas in the cell.