The Professional Induction Brazing Stainless Steel Tubing Joints Technology
The goal of this induction brazing application test is for Induction Brazing Stainless Steel Tubing Joints evenly for increased repeatability.
Industry:ย Automotive
Equipment:ย DW-UHF-10KW induction brazing machine
Time: 15 sec.
Materials: Stay Silv Black Flux
Temperature:ย 1472ยฐFย (800ยฐC)
Power: 8 kW
Process:
The two stainless tubes where joined together and an alloy ring was placed around the joint. Black flux was then applied to the joint for a better induction brazing process. The work piece was placed inside the helical coil for 15 seconds where 8 kW of induction heating power was applied. The work piece reached 1472ยฐFย (800ยฐC) and was successfully brazed.ย The HLQ induction heating equipment recommend for this application is the ย DW-UHF-10KW induction brazing heater along with aย 10 kW power supply.